Transback Endless Backing

Materials

Transback endless backings

No overlap joint delamination, no adhesive layer to be attacked or degraded, no compromise on food quality or medical applications

Material Backed belts – Description Abrasion
Resist
Coefficient
of friction
Temp
Range
Stress
Rating
This 95% natural rubber has outstanding resilience and remarkable cut and tear resistance. Excellent wet abrasion resistance. 5 0.7 +70°C
– 40°C
MSM
Reinforced natural and synthetic rubber with superior strength and resilience for severe abrasion resistance. Low compression set and high elasticity. 6 0.7 +70°C
– 40°C
HSM
Heavy duty reinforced natural and synthetic rubber mix with superior strength and resilience for severe abrasion resistance. Low compression set and high elasticity. 7 0.4 +80°C
– 30°C
HSM
White nitrile rubber suitable for most food and medical use including fatty foods. FDA Approved. Good heat aging resistance. 5 0.6 +80°C
– 60°C
MSM
This Synthetic rubber has outstanding resilience and remarkable cut and tear resistance. Excellent wet abrasion resistance. 5 0.7 +70°C
– 40°C
MSM
Reinforced natural and synthetic rubber with superior strength and resilience for severe abrasion resistance. Low compression set and high elasticity 7 0.7 +70°C
– 40°C
HSM
Silicon rubber with good release, wear/abrasion and temperature resistance (+200°C) properties. Non-toxic food and medical quality to FDA 177.2600. 7 0.4 +200°C
– 40°C
HSM
Silicon rubber with good release, wear/abrasion and temperature resistance (+200°C) properties. Non-toxic food and medical quality to FDA 177.2600. 7 0.4 +200°C
– 30°C
HSM